·滚防静电底漆
·铺设导电铜箔并做接地
·刮防静电砂浆中涂
·镘涂防静电腻子
·滚涂或喷涂防静电薄涂面漆
Construction Techniques:
·Ground or wall surface treatment.
·Coating conductive primer.
·Lay grounding copper line.
·Fill the seams the copper line leaves with conductive putty.
·Coat intermediate paint.
·Spray anti-static finished paint.
Technical Index :
测试项目 Test Items |
指标 Index |
表干h Surface Dry (h) |
≤4 |
实干h Actual Dry(h) |
≤24 |
附着力(级) Adhesion (Class) |
≤2 |
铅笔硬度(H) Pencil Rigidity(H) |
≥2 |
耐冲击性(Kg) Impact Resistance(Kg) |
50通过 50 Passed |
耐弯曲性 Folding Resistance |
1mm通过 1mm Passed |
柔韧性 Flexibility |
1mm通过 1mm Passed |
耐磨性(750g/500r,失重,g) Wear Resistance (750g/500rWeightlessness, g) |
≤0.02 |
耐水性 Water Resistance |
48小时无变化 No change for 48h |
耐10% H2SO4 H2SO4 10% Resistance |
56天无变化 No change for 56 days |
耐10% NaOH NaOH 10% Resistance |
56天无变化 No change for 56 days |
耐汽油,120# 120#Gasoline Resistance |
56天无变化 No change for 56 days |
耐热性 Heat Resistance |
2小时无变化 No change for 2h |
耐低温 Low Temperature Resistance |
-40℃ |
表面电阻(Ω) Surface Impedance (Ω) |
106-109 |
体积电阻(Ω) Volume Impedance(Ω ) |
106-109 |
1.恒久不变的防静电功能
2.镜面般光滑的表面
3.抗压耐磨,寿命持久
4.可承受中型荷载
缺点;
1.色彩没有防静电自流平地坪饱满
2.使用年限都没有耐磨地坪时间长;
1.防静电坪地施工完毕后需养护2-3天后方可投入使用,在养护期间,应避免水或其它溶液侵润表面
2.凡进入车间员工必须要换成胶底鞋
3.凡是硬件:如铁椅、铁桌,须将其脚用软质塑料、像胶包裹或用纸皮垫起来以免在使用过程中划伤地面
4.可根据地面要求做打蜡处理
混凝土裂缝修补方法:
1.表面修补:
表面修补法是一种简单,常见的修补方法,它主要适用于稳定和对结构承载能力,没有影响的表面裂缝以及深进裂缝处理。通常的处理措施是在裂缝的表面涂抹水泥浆,环氧胶泥或在混凝土表面涂刷油漆。在防护的同时为了防止混凝土受各种作用的影响继续开裂,通常可以采用在裂缝的表面黏贴玻璃纤维布等措施。
裂缝处理
1.如裂缝是由于结构本身的问题而产生的结构受力裂缝,要对结构进行加固补强修复,如裂缝为非结构受力裂缝。