性能项目 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
||
物理性能 |
比重 |
ASTM D792 |
2.30 |
|||
模塑收缩率 |
- |
流动方向 |
ASTM D955 |
7-9 |
||
- |
垂直方向 |
ASTM D955 |
7.59 |
|||
熔体流动速率 |
ASTM D1238 |
11.0 |
g/10min |
|||
机械性能 |
断裂拉伸强度 |
ASTM D638 |
5800 |
psi |
||
断裂伸长率 |
ASTM D638 |
6.0 |
% |
|||
断裂挠曲强度 |
ASTM D790 |
8000 |
psi |
|||
Izod缺口冲击强度 |
- |
无缺口 |
ASTM D4812 |
10 |
ft-lb/in |
|
- |
缺口 |
ASTM D256 |
1.5 |
ft-lb/in |
||
热性能 |
热变形温度 |
- |
66psi |
ASTM D648 |
400 |
℉ |
- |
264psi |
ASTM D648 |
315 |
℉ |
||
阻燃性 |
UL94 |
HB |